A complete list of stainless steel, which is good steel, 201, 202, 301, 302, or 304!
Stainless steel can be seen everywhere in daily life, and there are various models that are foolishly difficult to distinguish. Today, the editor will share an article with you to clarify the knowledge points inside.
Stainless steel is the abbreviation for stainless and acid resistant steel. Steel that is resistant to weak corrosive media such as air, steam, water, or has rust resistance is called stainless steel; And the type of steel that is resistant to chemical corrosion media (such as acid, alkali, salt, etc.) is called acid resistant steel. Stainless steel refers to steel that is resistant to weak corrosive media such as air, steam, water, and chemical corrosive media such as acid, alkali, and salt, also known as stainless acid resistant steel. In practical applications, steel that is resistant to weak corrosion media is often referred to as stainless steel, while steel that is resistant to chemical media corrosion is referred to as acid resistant steel. Due to the differences in chemical composition between the two, the former may not necessarily be resistant to chemical media corrosion, while the latter generally has rust resistance. The corrosion resistance of stainless steel depends on the alloying elements contained in the steel.
Common classification: usually classified by metallographic structure: usually, according to metallographic structure, ordinary stainless steel is divided into three categories: austenitic stainless steel, ferritic stainless steel, and martensitic stainless steel. On the basis of these three basic metallographic structures, dual phase steel, precipitation hardening stainless steel, and high alloy steel with iron content below 50% have been derived for specific needs and purposes. 1. Austenitic stainless steel. The matrix is mainly composed of austenite structure (CY phase) with a face centered cubic crystal structure, which is non-magnetic and mainly strengthened (and may lead to certain magnetism) by cold working in stainless steel. The American Iron and Steel Institute uses numbers from the 200 and 300 series, such as 304.
2. Ferritic stainless steel. The matrix is mainly composed of ferrite with a body centered cubic crystal structure (phase a), which is magnetic and generally cannot be hardened by heat treatment. However, cold work can slightly strengthen stainless steel. The American Steel Institute identifies 430 and 446.
3. Martensitic stainless steel. A stainless steel with a matrix of martensitic structure (body centered cubic or cubic), magnetic properties, and adjustable mechanical properties through heat treatment. The American Steel Institute is indicated by numbers 410, 420, and 440. Martensite has an austenitic structure at high temperatures, and when cooled to room temperature at an appropriate rate, the austenitic structure can transform into martensite (i.e. hardened). 4. Austenitic ferrite (duplex) type stainless steel. The matrix contains both austenite and ferrite phases, with a content of less than 15% in the matrix. It is magnetic and can be strengthened by cold working. 329 is a typical duplex stainless steel. Compared with austenitic stainless steel, duplex steel has higher strength, significantly improved resistance to intergranular corrosion, chloride stress corrosion, and pitting corrosion.
5. Precipitation hardening stainless steel. Stainless steel with a matrix of austenite or martensite structure that can be hardened by precipitation hardening treatment. The American Iron and Steel Institute uses numbers from the 600 series, such as 630, which is 17-4PH. Generally speaking, besides alloys, austenitic stainless steel has excellent corrosion resistance. In environments with low corrosion, ferritic stainless steel can be used. In mildly corrosive environments, if high strength or hardness is required, martensitic stainless steel and precipitation hardening stainless steel can be used. Characteristics and uses
Thickness differentiation 1: Because during the rolling process of steel mill machinery, the rolling rollers undergo slight deformation due to heating, resulting in a deviation in the thickness of the rolled plate. Generally, the middle is thick and the two sides are thin. When measuring the thickness of the board, the national regulations stipulate that the middle part of the board head should be measured.
2. The reasons for the occurrence of tolerances are generally divided into large tolerances and small tolerances based on market and customer needs: for example
What type of stainless steel is less prone to rusting?
There are three main factors that affect stainless steel corrosion:
1. The content of alloying elements. Generally speaking, steel with a chromium content of 10.5% is less prone to rusting. The higher the content of chromium and nickel, the better the corrosion resistance. For example, 304 material requires a nickel content of 8-10% and a chromium content of 18-20%. Such stainless steel will not rust under normal circumstances.
2. The smelting process of production enterprises can also affect the corrosion resistance of stainless steel. Large stainless steel plants with good smelting technology, advanced equipment, and advanced processes can ensure the control of alloy elements, removal of impurities, and control of cooling temperature of steel billets. Therefore, the product quality is stable and reliable, with good internal quality and less prone to rusting. On the contrary, some small steel mills have outdated equipment and processes. During the smelting process, impurities cannot be removed, and the products produced will inevitably rust.
3. The external environment is dry and well ventilated, making it less prone to rusting. Areas with high air humidity, continuous rainy weather, or high acidity and alkalinity in the air are prone to rusting. 304 stainless steel can also rust if the surrounding environment is too poor.
How to deal with rust spots on stainless steel?
1. In chemical method, acid cleaning paste or spray is used to assist the rusted parts to passivate again and form chromium oxide film to restore their corrosion resistance. After acid cleaning, in order to remove all pollutants and acid residues, it is very important to properly rinse with clean water. After all processing, use polishing equipment to re polish and seal with polishing wax. For areas with slight rust spots, a 1:1 mixture of gasoline and engine oil can be used to wipe off the rust spots with a clean cloth.
2. Mechanical sandblasting, shot blasting with glass or ceramic particles, immersion, brushing, and polishing. It is possible to use mechanical methods to wipe away contamination caused by previously removed materials, polishing materials, or annihilated materials. All kinds of pollution, especially foreign iron particles, can become a source of corrosion, especially in humid environments. Therefore, it is best to perform formal cleaning on mechanically cleaned surfaces under dry conditions. The use of mechanical methods can only clean the surface and cannot alter the corrosion resistance of the material itself. Therefore, it is recommended to re polish with polishing equipment after mechanical cleaning and seal with polishing wax.
Commonly used stainless steel grades and performance for instruments
1. 304 stainless steel. It is one of the most widely used and widely used austenitic stainless steels, suitable for manufacturing deep drawing formed parts, acid pipelines, containers, structural components, various instrument bodies, etc. It can also be used to manufacture non-magnetic and low-temperature equipment and components.
2. 304L stainless steel. In order to address the serious intergranular corrosion tendency of 304 stainless steel caused by the precipitation of Cr23C6 under certain conditions, ultra-low carbon austenitic stainless steel has significantly better intergranular corrosion resistance in its sensitized state than 304 stainless steel. Except for slightly lower strength, other properties are the same as 321 stainless steel, mainly used for corrosion-resistant equipment and components that require welding but cannot undergo solid solution treatment. It can be used to manufacture various instrument bodies, etc.
3. 304H stainless steel. The internal branch of 304 stainless steel has a carbon mass fraction between 0.04% and 0.10%, and its high-temperature performance is superior to that of 304 stainless steel.
4. 316 stainless steel. Adding molybdenum on the basis of 10Cr18Ni12 steel gives the steel good resistance to reducing media and pitting corrosion. In seawater and various other media, the corrosion resistance is better than 304 stainless steel, mainly used as a corrosion-resistant material.
5. 316L stainless steel. Ultra low carbon steel has good resistance to intergranular corrosion in sensitized state, and is suitable for manufacturing welded components and equipment with thick cross-sectional dimensions, such as corrosion-resistant materials in petrochemical equipment.
6. 316H stainless steel. The internal branch of 316 stainless steel has a carbon mass fraction between 0.04% and 0.10%, and its high-temperature performance is better than that of 316 stainless steel.
7. 317 stainless steel. The resistance to pitting corrosion and creep is superior to 316L stainless steel, used in the manufacturing of petrochemical and organic acid corrosion resistant equipment.
8. 321 stainless steel. Titanium stabilized austenitic stainless steel, with the addition of titanium to improve intergranular corrosion resistance and excellent high-temperature mechanical properties, can be replaced by ultra-low carbon austenitic stainless steel. Except for special occasions such as high temperature or hydrogen corrosion resistance, it is generally not recommended to use.
9. 347 stainless steel. Austenitic stainless steel stabilized with niobium can improve its intergranular corrosion resistance by adding niobium. Its corrosion resistance in corrosive media such as acid, alkali, and salt is the same as that of 321 stainless steel. It has good welding performance and can be used as both a corrosion-resistant material and a heat-resistant steel. It is mainly used in the fields of thermal power and petrochemicals, such as making containers, pipelines, heat exchangers, shafts, furnace tubes in industrial furnaces, and furnace tube thermometers.
10. 904L stainless steel. Super fully austenitic stainless steel is a type of super austenitic stainless steel invented by OUTOKUMPU company in Finland. Its nickel mass fraction is 24% -26%, and carbon mass fraction is less than 0.02%. It has excellent corrosion resistance and excellent resistance to non oxidizing acids such as sulfuric acid, acetic acid, formic acid, and phosphoric acid. It also has good resistance to crevice corrosion and stress corrosion. Suitable for various concentrations of sulfuric acid below 70 ℃, it has good corrosion resistance in any concentration and temperature of acetic acid and a mixture of formic acid and acetic acid under normal pressure. The original standard ASMESB-625 classified it as nickel based alloy, while the new standard classified it as stainless steel. China only has similar grades of 015Cr19Ni26Mo5Cu2 steel, and a few European instrument manufacturers use 904L stainless steel as their key material. For example, the measuring tube of the E+H mass flow meter is made of 904L stainless steel, and the case of Rolex watches is also made of 904L stainless steel. 11. 440C stainless steel. Martensitic stainless steel has the highest hardness among hardenable stainless steel and stainless steel, with a hardness of HRC57. Mainly used for making nozzles, bearings, valve cores, valve seats, sleeves, valve stems, etc.
12. 17-4PH stainless steel. Martensitic precipitation hardening stainless steel, with a hardness of HRC44, has high strength, hardness, and corrosion resistance, and cannot be used at temperatures above 300 ℃. It has good corrosion resistance to the atmosphere and diluted acids or salts, and its corrosion resistance is the same as 304 stainless steel and 430 stainless steel. It is used for manufacturing offshore platforms, turbine blades, valve cores, valve seats, sleeves, valve stems, etc.
In the field of instrumentation, considering universality and cost issues, the conventional selection order for austenitic stainless steel is 304-304L-316-316L-317-321-347-904L stainless steel. 317 is less commonly used, 321 is not recommended, 347 is used for high-temperature corrosion resistance, and 904L is only the default material for some components from individual manufacturers. 904L is generally not actively selected in design. In the design and selection of instruments, there are usually situations where the material of the instrument is different from that of the pipeline, especially in high-temperature working conditions. Special attention should be paid to whether the selection of instrument materials meets the design temperature and pressure of the process equipment or pipeline. For example, if the pipeline is made of high-temperature chromium molybdenum steel and the instrument is made of stainless steel, there may be problems, and it is necessary to consult the temperature and pressure gauges of the relevant materials.
In instrument design and selection, various stainless steels of different systems, series, and grades are often encountered. When selecting, multiple perspectives such as specific process media, temperature, pressure, stress components, corrosion, and cost should be considered.